The smallest etch rate and best anisotropic profiles were obtaine

The smallest etch rate and best anisotropic profiles were obtained with the SF6/CHF3 gas mixture. Using a PAA mask

with highly ordered hexagonally arranged nanopores, a perfect pattern transfer of the nanopores to a large Si area is achieved. The same is possible on small pre-defined areas on the Si SC79 manufacturer wafer. Authors’ information VG and AO are post-doctoral researchers. AGN is the director of research at NCSR Demokritos/IMEL and the head of the “Nanostructures for Nanoelectronics, Photonics and Sensors” research group. Acknowledgments This work was partially financed by the 03ED375 PENED research project with funds from the Greek Ministry of Development (80%) and EU (20%). Funding was also received from the European Community’s Seventh Framework Programme (FP7/2007-2013) under grant agreement NANOFUNCTION n°257375.

References 1. Asoh H, Sasaki K, Ono S: Electrochemical etching of silicon through anodic porous alumina. see more Electrochem Commun 2005, 7:953–956.CrossRef 2. Crouse D, Lo YH, Miller AE, Crouse M: Self-ordered pore structure of anodized aluminum on silicon and pattern transfer. Appl Phys Lett 2000, 76:49–51.CrossRef 3. Zacharatos F, Gianneta V, Nassiopoulou AG: Highly ordered hexagonally arranged nanostructures on silicon through ACY-738 cost a self-assembled silicon-integrated porous anodic alumina masking layer. Nanotechnology 2008, 19:495306.CrossRef 4. Zacharatos F, Gianneta V, Nassiopoulou AG: Highly ordered hexagonally arranged sub-200 nm diameter vertical

cylindrical pores on p-type Si using non-lithographic pre-patterning of the Si substrate. Phys Status GPX6 Solidi A 2009, 206:1286–1289.CrossRef 5. Hourdakis E, Nassiopoulou AG: High performance MIM capacitor using anodic alumina dielectric. Microelectron Eng 2012, 90:12–14.CrossRef 6. Hourdakis E, Nassiopoulou AG: High-density MIM capacitors with porous anodic alumina dielectric. IEEE Trans Electron Dev 2010,57(10):2679–2683.CrossRef 7. Huang GH, Lee EJ, Chang WJ, Wang NF, Hung CI, Houng MP: Charge trapping behavior of SiO 2 -Anodic Al 2 O 3 –SiO 2 gate dielectrics for nonvolatile memory applications. Solid State Electron 2009, 53:279–284.CrossRef 8. Hourdakis E, Nassiopoulou AG: Charge-trapping MOS memory structure using anodic alumina charging medium. Microelectron Eng 2011,88(7):1573–1575.CrossRef 9. Masuda H, Fukuda K: Ordered metal nanohole arrays made by a two-step replication of honeycomb structures of anodic alumina. Science 1995, 268:1466–1468.CrossRef 10. Li AP, Birner A, Nielsch K, Gösele U: Hexagonal pore arrays with a 50–420 nm interpore distance formed by self-organization in anodic alumina. J Appl Phys 1998, 84:6023–6026.CrossRef 11. Lee W, Ji R, Gösele U: Fast fabrication of long-range ordered porous alumina membranes by hard anodization. Nat Mater 2006, 5:741–747.CrossRef 12.

Comments are closed.